- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Okay with tool coating
Thermal diffusion extends stamping die life, reduces press downtime
- By Todd Earl
- November 8, 2005
- Article
- Bending and Forming
Applying a thermal diffusion coating to stamping tooling has doubled tool life. Production runs now exceed 100,000 cycles, according to the company. |
In the 35 years Okay Industries, New Britain, Conn., has been in the stamping business, it has grown to 160 employees, including 11 tool designers/engineers and 25 toolmakers. The stamper uses all 100 of its 10-ton to 800-ton presses in its 100,000-square-foot facility.
Okay serves diverse market segments, including medical, automotive, electronics, defense, and specialty industrial.
The precision stamper likes to take on the tough jobs—the ones other companies don't want. However, those tough jobs came with a price tag in the form of high die maintenance costs caused by high wear or galling, excessive press downtime, and overuse of lubricants.
Converting Cast Components to Stampings
The stamper produces a roller finger follower for automotive applications. The part is made of 0.098-inch-thick 1008 cold-rolled steel.
The traditional method of manufacturing the roller finger follower was to cast it and then run it through secondary operations such as boring, grinding, and lapping. The part performed satisfactorily, but the high cost needed to be reduced, especially since engines were being designed with more valves.
So the automotive industry had it remanufactured as a stamped and formed (flanged) part to reduce cost.
However, this design had several disadvantages. The component was heavier and less stiff than the cast version, which had an adverse impact on fuel economy and emissions. In addition, flanges were thicker than the cast version. Finally, the stamped component required a clip assembly in the socket area for final assembly into the engine, which also increased costs.
Okay partnered with its customer to understand the critical requirements of the application and developed (and joint-patented) a method for manufacturing a lower-cost stamped roller finger follower that was lighter, narrower, and stronger: stamping and forward extruding it into the same configuration as a cast part. The part could be net-shape stamped, heat-treated, and shipped to the customer without adding additional components or secondary operations.
Thermal diffusion is a hot process that combines carbon from the tool surface with vanadium to grow a vanadium/ultradense carbide layer that is bonded to the substrate metallurgically. |
A Solution Prompts Another Problem
There were many challenges to developing this version of a stamped roller finger follower, however. One was creating valve stem guide side walls long enough so the parts would not tip over during assembly. The stamper addressed this challenge by forward-extruding material into a die cavity that produced net-shape valve guide side walls to keep the valve stem aligned during assembly.
While this process worked, the forces involved fractured the tooling components after only a few parts were produced. "In this die, we have stations that blank, pierce, and form the part," said Jim DeVecchis, design engineer. "In the forming stations we are pushing the metal around in a small radius and the material wants to slide. As a result, we experience extreme heat and galling in these areas. This condition will distort the part and wear down the tool at an unacceptable rate," he said.
To achieve an acceptable tool life, the stamper engineered a tooling concept that prestressed the tool components by heating retainers and supercooling die components. When assembled together, the retainers and die inserts return to ambient temperature, causing the retainers to shrink and the die inserts to expand. This robust design increased the rupture strength for tooling components to 50,000 cycles.
In an effort to extend tool life even more, the stamper applied a thermal diffusion process coating from TD Center, Columbus, Ind., to the tool components.
Thermal Diffusion Tool Coating
Thermal diffusion is a hot process (1,800 degrees F) that combines carbon from the tool surface with vanadium to grow a vanadium/ultradense carbide layer—0.0002 to 0.0003 in. thick with a hardness of 3,500 to 3,800 Vickers hardness, well above 90 Rockwell C—that is bonded to the substrate metallurgically.
This method creates a bond stronger than deposited coatings, according to TD Center. The coating is durable, will not chip or peel off the substrate, and provides good abrasive wear protection.
Applying the thermal diffusion process to the tooling has doubled tool life and, subsequently, production runs, which now exceed 100,000 cycles, DeVecchis said.
"There are 14 stations on the die. The TD process is used on three of them," DeVecchis said. "It has given us better product quality, less scrap, faster throughput, longer die life, and reduced die dressing."
Reduced, Changed Lubricant Usage
"We have changed over our lubrication to a nontoxic oil and coolant," DeVecchis said. He added, "Because of the TD process, we can use a water-based coolant for many of our dies. Otherwise, more expensive coolant or oils would have to be used. In areas of the die where the part normally would run hot, the coolant significantly reduces the heat. Now with the TD process and our new water-based coolant, we have a part coming off that you can pick up."
The company has applied the thermal diffusion coating process to other stamped components as well. Almost all of Okay's new dies now have a thermal diffusion coating specified for them, DeVecchis said. "They are used primarily for areas of high wear or galling and to reduce lube costs, especially for drawn parts."
Okay Industries Inc., 200 Ellis St., New Britain, CT 06051, 860-225-8707, fax 860-225-7047, www.okayind.com
TD Center, 2020 15th St., Columbus, IN 47201, 877-832-3687, fax 812-378-1591, www.tdcoating.com
About the Author
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
White House considers China tariff increases on materials
A visit to Automate 2024 reveals the future might be now
Majestic Steel Arkansas fully operational
Rivian to expand Illinois facility to manufacture midsized SUV
Why employee-owned companies make sense in manufacturing
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,