President
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Aluminum Workshop: Electrical current in TIG and MIG
- By Frank Armao
- December 11, 2014
- Article
- Aluminum Welding
Q: When I gas tungsten arc weld (GTAW) aluminum, I always use alternating current (AC), but when I gas metal arc weld (GMAW) aluminum, I always use direct current electrode positive (DCEP). Why the difference? Does anyone GTAW aluminum using DC? Does anyone GMAW using AC?
A: In both GTAW and GMAW, if you use EP, you put about 70 percent of the arc energy into the tungsten electrode or GMAW filler wire, and if you use electrode negative, you put about 70 percent of the arc energy into the work.
In GTAW, you want to minimize the energy going into the tungsten electrode so it doesn’t melt. That’s why you use DCEN to GTAW most materials.
Additionally, in GTAW, DECEN maximizes weld penetration. However, when welding aluminum, you find that DCEP actually removes the oxide from the aluminum surface, making it easier to weld. Many years ago someone figured that if you use AC to weld aluminum, you get the arc cleaning you need from the EP part of the AC cycle, and you get the penetration you want from the EN part of the AC cycle.
Can you GTAW aluminum using DCEN? Yes. However, you don’t get any oxide removal from the arc cleaning, so preweld cleaning requirements are much more stringent. For this reason, DCEN GTAW is somewhat of a specialty process and isn’t common.
The situation is different with GMAW, in which you get both oxide removal and penetration from the DCEP current. If you used DCEN to GMAW aluminum, you would get no oxide removal and very little penetration. So really no good reason exists to use DCEN for GMAW. (Yes, I know that some FCAW electrodes are welded using DCEN, but we’re talking aluminum here.)
Actually, a few specialty AC GMAW power sources for aluminum can be found on the market. They are used primarily for welding very thin aluminum. In this case, adding a bit of EN current to the EP will actually cut down the weld penetration, which can be very helpful in the thin material. However, these power supplies tend to be complex and very expensive, and as a result they are not commonly seen.
About the Author
Frank Armao
Aluminum Consulting Inc.
440-479-0239
About the Publication
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
The role of flux in submerged arc welding performance
Aluminum MIG wires offer smooth feeding, reduced tangling
Connecticut students compete in Maritime Welding Competition
Welding power source’s modes designed to help optimize performance
Building a successful welding program from the ground up
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,