President
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Aluminum Workshop: How to Identify Aluminum Types
- By Frank Armao
- Updated August 8, 2023
- December 10, 2014
- Article
- Aluminum Welding
A: This is a good question and one to which there is no easy answer. There is no quick, cheap test that will tell you which aluminum alloy you have. Some equipment can perform chemical analysis without destroying the part, but it is very expensive. The best I can do is provide you with guidelines.
Types of Aluminum Alloys
Castings. While there are many different types of aluminum casting alloys available, the most common castings you will encounter are AlSiMg alloys. The best filler metal for these alloys is 4043.
Extrusions.Extrusions should be easy to recognize. Anything that is an open section, such as an angle or channel shape, or a closed section, such as a round tube or more complex section, is probably an extrusion. Solid shapes, such as round or square bar, can be extruded as well. If you look at the surface of an extrusion, you should see a pattern of fine lines along the long axis. These result from the extrusion process. Aluminum extrusions made In North America or Europe are almost always 6061, 6063, 6082, or 6005. All of these alloys can be welded easily using 4043 or 5356. However, extrusions made in Asia usually are made from 7005, an AlZnMg alloy. You can be fairly sure the extrusions are 7005 if you are working on a motorcycle, bicycle, or car made in Japan or China. The preferred filler for this alloy is 5356.
Bar. Most solid shapes, such as rod or squares, are made by rolling bar. In North America, these are most often made from 6XXX alloys and can be welded using 4043 or 5356 filler.
Sheet and Plate. The most common sheet and plate alloys in North America are the 3XXX and 5XXX series, for which 5356 filler is preferred. However, 6061 is commonly available as a plate alloy, as are the 2XXX and 7XXX alloys, which should not be welded because most of them are considered unweldable.
There is really no easy test to find out which sheet or plate alloy you have.
About the Author
Frank Armao
Aluminum Consulting Inc.
440-479-0239
About the Publication
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
The role of flux in submerged arc welding performance
Aluminum MIG wires offer smooth feeding, reduced tangling
Building a successful welding program from the ground up
Connecticut students compete in Maritime Welding Competition
Welding power source’s modes designed to help optimize performance
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,