President
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Aluminum Workshop: Preventing porosity in humid environments
- By Frank Armao
- March 11, 2008
- Article
- Aluminum Welding
Q: I'm having problems with excessive porosity when TIG welding aluminum. My friend says it comes from water vapor in the air (it's very humid here) being broken down by the arc. Is this true? It sounds pretty far-fetched.
A: I hope you didn't bet on this one. If you did, get ready to pay up. All porosity in aluminum welds is caused by hydrogen. Liquid aluminum can dissolve a lot of hydrogen, but solid aluminum can dissolve almost no hydrogen. So a molten aluminum weld sucks up any hydrogen around. As it solidifies, the weld tries to get rid of the hydrogen. If it can, everything is OK. If it can't, you get porosity.
So where does the hydrogen come from? Basically, there are two sources. The first is any sort of hydrocarbon, like oils, greases, and solvents. The second is water vapor. The temperature in a welding arc is more than 10,000 degrees F, hot enough to break down these substances into hydrogen plus something else.
So how do you minimize porosity in aluminum welds? First, clean the aluminum with a good degreaser, and make sure the solvent has completely evaporated before you weld. Check that there are no water or air leaks in the torch or cables. Close all nearby windows and doors so there are no breezes (even a slight breeze can deteriorate the shielding gas coverage and suck moist air into the arc). If you brought your base metal in from outside, make sure there is no water condensation on it. You need to look at lots of other things too, but they all fall into the housekeeping category. If you take care of these during weld preparation, your job will be a lot easier.
As for welding in very humid conditions, I must admit that high humidity does make it more difficult to make porosity-free welds. However, this is usually because your housekeeping has gotten sloppy. If you return to basics and complete the necessary weld preparation, you should be able to make porosity-free welds even at very high levels of humidity.
About the Author
Frank Armao
Aluminum Consulting Inc.
440-479-0239
About the Publication
Related Companies
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Connecticut students compete in Maritime Welding Competition
Welding power source’s modes designed to help optimize performance
Building a successful welding program from the ground up
Torch made for welding thin, conductive sheet metal
Welding jacket designed for protection, comfort
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,