Press Brake Tooling Buyers' Guide



American Style European Style OEM-Specific Surface Finish Precision-Ground Coefficient of Friction Inches Coefficient of Friction MM Surface Treatment
Process or Name Hardness Optional

LVD Strippit  Akron, NY

.5 .4 .0004 .01 Induction 57 S

TRUMPF Inc.  Farmington, CT

.0004 .01 LASERdur Deep Hardening 62 - 64 S

Atek Corp.  Kewanee, IL

30 O

Fab Supply Inc.  Addison, IL

O

Mecon Industries  Toronto, ON Canada

          29-60

Press Brake Tooling Corp.  Addison, IL

    .0008 .02    30-55

Unittool Punch & Die Co. Inc.  Buffalo, NY

O

Wila USA  Hanover, MD

.0004 .01 CNC-Deep hardening 56 - 60 S
           

Wilson Tool International® Inc.  White Bear Lake, MN

.25 15 .0008 .02 Nitrex/Laser Hardened 70/55-60 S
.005 .13 Induction 55-60 O
.25 15 .0008 .02 Nitrex/Laser Hardened 70/55-60 S
.25 15 .0004 .01 Nitrex/Laser Hardened 70/55-60 S